This simple, easy-to-use gage measures the thickness of applied dry coating powder …before it’s been cured!
Check Powder thickness with Powder Comb before curing to help ensure correct cured film thickness the first time through the line. Avoid stripping and re-coating which can cause problems with adhesion and coating integrity.
Powder Comb Models |
Height Tooth 1 |
Height Tooth 2 |
Height Tooth 3 |
Height Tooth 4 |
---|---|---|---|---|
Model 1 (mils) | 3 | 6 | 9 | 12 |
Model 2 (mils) | 10 | 15 | 20 | 25 |
Model 3 (mils) | 20 | 30 | 40 | 50 |
Model 4 (μm) | 75 | 150 | 225 | 300 |
Model 5 (μm) | 250 | 375 | 500 | 625 |
Model 6 (μm) | 500 | 750 | 1000 | 1250 |
Versatility
Quality
Simple Operation
Example: The 75 and 150 micron teeth both make lines and have powder clinging to them but the 225 mil tooth does not. The uncured powder thickness is determined to be between 150 and 225 microns. (see above image)
Note – Most powders cure to approximately 50% of their dry thickness. Marks left by the gage may affect the characteristics of the cured film.
1550 Cobb Industrial Dr. | P.O. Box 9098 | Marietta, GA 30065-2098
770-425-1355 (Phone) | 770-425-1354 (Fax) | info@alliedcorrosion.com (Email)
Made with ❤ by Mighty Good Marketing
We care about your privacy! In order to run a successful website, we are setting cookies and accessing and storing information on your device for various purposes. By continuing to browse this site, you are agreeing to our use of cookies.
If you wish to disable cookies, please visit our Privacy Policy for more information.
Got It! Thanks!Privacy policy